喷涂成品在干燥固化期间,避免受到机械碰撞及雨水冲刷
添加时间:2023/6/1 16:20:43     浏览次数:
对喷涂后的保温吸声层,应提供通风、干燥环境,通常在平均温度25℃,相对湿度≤60%时,依据不同厚度干燥固化时间为24~72小时,此后可进行装饰等其他工序。
The heat absorption layer after spraying, should provide a dry and ventilated environment, usually in an average temperature of 25 degrees Celsius, relative humidity is less than 60%, according to the different thickness of drying and curing time for 24~72 hours, then decoration and other processes.
喷涂成品保护
Finished product protection
喷涂前应安装各种管线、风道等设备吊挂件,避免喷涂完工后在基面钻孔、剔凿。
Before spraying, all kinds of equipment such as pipeline and air duct should be installed to avoid drilling and picking on the base surface after spraying.
施工准备
Construction preparation
喷涂成品在干燥固化期间,避免受到机械碰撞及雨水冲刷。
Spray finished products during drying and curing period to avoid mechanical collision and rain erosion.
对于喷涂层局部因受到碰撞而造成破损时,应进行局部修补;对于经常处于容易受到机械碰撞的部位,可贴覆玻璃纤维布或其它地变电阻柜 精密铸造 中频电炉设备 保定断桥铝门窗 保定养老院 镜子批发 启闭机护材料,用以对纤维层表面进行保护。
For local coating caused by the collision damage, should be carried out for local repair; often vulnerable to mechanical impact part, can stick to glass fiber cloth or other protective materials used to protect the surface of the fiber layer.
上一页  喷涂成品保护及注意事项  
下一页  喷涂成品在干燥固化期间,避免受到机械碰撞及雨水冲刷。
  • 关于我们
  • 新闻动态
  • 案例展示
  • 网上订单
  • 联系我们
  • 产品分类1
  • 产品分类2
  • 产品分类3

Copyright © 技术支持:遨游网络

  • 联系我们
  • 网上订单
  • 工程案例
  • 本站导航

搜索

  • 关于我们
  • 新闻动态
  • 案例展示
  • 网上订单
  • 联系我们
  • 产品分类1
  • 产品分类2
  • 产品分类3